Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 6.50 g/cc | 6.50 g/cc | ASTM D792 |
Ecomass® 1850ZD88 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Specific Gravity | 6.50 g/cc | 6.50 g/cc | ASTM D792 |
Ecomass® 1850ZG90 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Specific Gravity | 6.50 g/cc | 6.50 g/cc | ASTM D792 |
Ecomass® 1850ZG92 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Specific Gravity | 6.50 g/cc | 6.50 g/cc | |
Parker Chomerics CHO-SHIELD® 1091 PRIMER CHO-SHIELD 1091 is an air-drying liquid coating for enhancing the adhesion of CHO-SHIELD 2001 and 2003 corrosion resistant, electrically conductive coatings to chemically treated aluminum. CHO-SHIEL.. |