Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.10 g/cc | 4.10 g/cc | |
Excalibar ExBar™ 200 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Specific Gravity | 4.10 g/cc | 4.10 g/cc | |
Excalibar ExBar™ 325 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Specific Gravity | 4.10 g/cc | 4.10 g/cc | |
Excalibar ExBar™ 400 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Specific Gravity | 4.10 g/cc | 4.10 g/cc | |
Excalibar NewWate™ Barite BaSO4 Powder NewWate™ barite is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas exploration. NewWate.. |
|||
Specific Gravity | 4.10 g/cc | 4.10 g/cc | |
DayGlo Phantom IPO-15 Invisible Pigment, Orange These materials have a yellowish or white color body under visible light and produce a bright vibrant color when exposed to an Ultra-Violet light source. Phantom pigments can be used for security an.. |
|||
Specific Gravity | 4.10 g/cc | 4.10 g/cc | |
DayGlo Phantom IPO-19 Invisible Pigment, Blue These materials have a yellowish or white color body under visible light and produce a bright vibrant color when exposed to an Ultra-Violet light source. Phantom pigments can be used for security an.. |