Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.438 g/cc | 3.438 g/cc | |
Indium Corp. In2(SO4)3 * 9H2O Indium Sulfate Hydrated Salt Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, an.. |
|||
Specific Gravity | 3.438 g/cc | 3.438 g/cc | |
Indium Corp. In2(SO4)3 Indium Sulfate Anhydrous Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, an.. |