Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.14 g/cc | 2.14 g/cc | Part A; TM R050-16 |
Resinlab® EP1121-4 Adhesive / Casting Resin Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives .. |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
3M Dyneon™ FEP X 6301 UHP Fluorothermoplastic Fluorinated Ethylene Propylene
(discontinued **) Dyneon FEP X 6301 UHP was designed primarily for ultra-high purity applications requiring very low levels of metals and ions. This extrusion grade of EEP is ideally suited for tubing, which can be u.. |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | ASTM D792 |
Technetics Group Texolon™ 7865 PTFE
(Unverified Data**) Virgin PTFE for those applications not requiring the premium qualities of 8764 sheet.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surfac.. |
|||
Specific Gravity | 2.14 - 2.17 g/cc | 2.14 - 2.17 g/cc | ISO 12086 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Specific Gravity | 2.14 - 2.19 g/cc | 2.14 - 2.19 g/cc | ASTM D792 |
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon. |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | ASTM D 792 |
Karina E 1000/HMB 21586 White Concentrate Color Concentrate Filled white concentrate designed for general purpose film applications based on olefin resins. Letdown ratio estimated from 1% to 5%.Information provided by Karina Indústria e Comércio de PlÃ.. |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | |
Garlock 8764 PTFE Rubber Sheet Premium Grade Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive.. |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | Part B |
Master Bond Super Gel 9AOND Dimensionally Stable Urethane Modified Epoxy Master Bond Super Gel 9AOND is a two component, urethane modified epoxy system that cures at room temperature and has a paste-like consistency. It offers softness and retains dimensional stability. .. |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive.. |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive.. |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive.. |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive.. |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive.. |
|||
Specific Gravity | 2.14 g/cc @Temperature 25.0 °C |
2.14 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 4446 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility.Information provided by Dow Corning |
|||
Specific Gravity | 2.14 - 2.16 g/cc | 2.14 - 2.16 g/cc | ASTM D792 |
Adamas Adalon® 301 PTFE, 10% Graphite Information provided by Adamas, HPM |
|||
Specific Gravity | 2.14 - 2.17 g/cc | 2.14 - 2.17 g/cc | ASTM D792 |
Adamas Adalon® 902 PTFE, 1% Conductive filler Information provided by Adamas, HPM |
|||
Specific Gravity | 2.14 - 2.18 g/cc | 2.14 - 2.18 g/cc | ASTM D792 |
Adamas Adalon® 991 PTFE Information provided by Adamas, HPM |
|||
Specific Gravity | 2.14 - 2.18 g/cc | 2.14 - 2.18 g/cc | ASTM D792 |
Adamas Adalon® 998 PTFE, Turquoise Information provided by Adamas, HPM |
|||
Specific Gravity | 2.14 g/cc | 2.14 g/cc | ASTM D792 |
3M Dyneon™ FEP 6301Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6301Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | ASTM D792 |
Technetics Group Texolon™ 8764 PTFE
(Unverified Data**) A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri.. |
|||
Specific Gravity | 2.14 - 2.17 g/cc | 2.14 - 2.17 g/cc | |
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |
|||
Specific Gravity | 2.14 - 2.16 g/cc | 2.14 - 2.16 g/cc | ASTM D792 |
Adamas Adalon® 305 PTFE, 15% Graphite Information provided by Adamas, HPM |