Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.83 g/cc | 1.83 g/cc | |
Omya OMYAFLOW® 3 - SY Calcium Carbonate A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Decorative paints.Information supplied by Omya North A.. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | ASTM D792 |
PolyOne Edgetek® SF-30GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | |
Kuraray HYBRAR® Blends Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | ASTM D792 |
Haysite SDL® H261 Polyester, Static Dissipative H261 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H261.. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | |
Silberline EternaBrite® Premier 351 EternaBrite® Premier 351 is a fine, very bright, lenticular leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This g.. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | ASTM D297, 15 |
Seals Eastern 7042 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | |
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi.. |
|||
Specific Gravity | 1.83 - 1.89 g/cc | 1.83 - 1.89 g/cc | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Specific Gravity | 1.83 g/cc | 1.83 g/cc | ASTM D792 |
Premix Premi-Glas® 1281-32 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1281-32 VE SMC is a high strength glass reinforced vinyl ester sheet molding compound formulated for under-the-hood automotive applications. Key features and benefits: Desi.. |