Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.76 g/cc | 1.76 g/cc | |
Old Hickory M&M Clays, Inc. Wilco-SLU Kaolin Clay Wilco SLU is an aqueous suspension of kaolin produced at 70% solids content. The slurry is deflocculated and rheology stabilized with sodium silicate. The Wilco SLU grade is a highly permeable selec.. |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | |
Silberline Sparkle Silver Ultraâ„¢ 6704 Sparkle Silver Ultraâ„¢ grades are very bright lenticular automotive aluminum pigments. They offer a very smooth patina and narrow particle size distribution, allowing the formulator to create ve.. |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | ASTM D792 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | ASTM D792 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | |
BCC Products BC 6060 Epoxy Surface Coat/Casting BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum.. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Specific Gravity | 1.76 - 1.78 g/cc | 1.76 - 1.78 g/cc | ASTM D792 |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Adamas Adalon® 451 PTFE, organic filler Information provided by Adamas, HPM |
|||
Specific Gravity | 1.76 g/cc | 1.76 g/cc | Method A; ASTM D792 |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |