Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Ovation Polymers Opnyl OP66GF60 Nylon 66, 60% Glass Reinforced Nylon 66 - Glass reinforced (60 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared.. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var.. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH
(disco AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | 73°F; ASTM D792 |
Matrixx Group 84S7301 Flame Retardant 30% Glass Reinforced PET (V0)
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | |
Kuraray Genestarâ„¢ GA2330 Nylon, 33% Glass Filled Abrasion Resistance V-0 Grade. Can be used for applications requiring high abrasion and heat resistance, as well as flame retardancy, such as internal gear of copying machine. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12 LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | |
BCC Products BC 4570 Polyester Hi Heat Filler BC 4570 is a multi-purpose paste designed for making quick repairs to a variety of substrates where service temperature exceeds 200º F (93º C). It is easy to mix and apply, cures in 15-20 minutes .. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa.. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry
(discontinued **) Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
Custom Resins Vexel™ E20GF30 FR , 30% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF30 FR is a 30% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |