Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
Custom Resins Vexel™ E20MG35 , 35% Glass/Mica Reinforced PET
(discontinued **) Description: Vexel™ E20MG35 is a 20% glass fiber / 15% mica reinforced PET. Information provided by Custom Resins. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R1212A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp
(discontinued **)< Information provided by PolyOne™ Corporation |
|||
Specific Gravity | 1.61 g/cc @Temperature 23.0 °C |
1.61 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa PBT-RG302 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® GP-5400G PBT, 40% Glass Filled Material with 40% GF reinforcement that is used in motor insulatorsInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | |
Silberline SparkleBriteâ„¢ Premier 2200NL-PA SparkleBriteâ„¢ Premier pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced metallic effects in s.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Grey 8368 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8368 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Grey 8368 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8368 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White HS8350 Concentrate Based In Impact Polystyrene DescriptionPOLYBATCH® HS8350 is a white masterbatch containing 50% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive .. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | |
Trelleborg R661 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White HS8350 Concentrate Based In Impact Polystyrene DescriptionPOLYBATCH® HS8350 is a white masterbatch containing 50% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive .. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall EX 3154 Plenum Flexible PVC Non-lead stabilized CAT 3 plenum jacket. Recommended for up to 25 pair, unshielded.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall 02541 Plenum Flexible PVC Non-lead stabilized CAT 3 jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |