Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
PolyOne Nymax™ ND 1233 GF Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D792 |
S&E Specialty Polymers GPE2001F-ROHS PVC Application: GPE2001F-ROHS is flame retardant polyethylene compound designed for wire and cable applications. GPE2001F-ROHS complies with RoHS requirements. GPE2001F-ROHS is suitable for 75°C cont.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
S&E Specialty Polymers TufFill NH™ GTPO8290-36 TPO Application: A 105°C rated, Flexible, TPO based, Zero Halogen compound, exhibiting excellent processing characteristics with superior physical and low temperature propertiesInformation provided by .. |
|||
Specific Gravity | 1.39 - 1.41 g/cc | 1.39 - 1.41 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET B-113C PET Sheet Grade Used mainly for box strapping. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D1638 |
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid) Interior application for thick & thin gauge profile application.Information provided by PolyOne |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R100AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | Mixed; TM R050-16 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D3763 |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12
(discontinued **) Information provided by PolyOne Corporation. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Kolon KOCETAL® LF301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | |
Momentive Performance Materials FSE7540 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ISO 1183 |
Lanxess Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | |
Sylvin Technologies 9980-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Teknor Apex APEX® 4157 Polyvinyl Chloride Compound Notes: Non-Migrating; Sunlight Resistant, Tray Cable Jacket Temperature Rating: 105°CInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Teknor Apex APEX® 536 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4535 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 4535 is a blue color concentrate based in polyethylene . This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 4535 is typi.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | |
Trelleborg P600 Epichlorohydrin There are three types of epichlorohydrin:1. Homopolymers of epichlorohydrin. Designated CO.2. Chopolymers of epichlorohydrin and etylene oxide. Designated ECO.Terpolymers of epichlorohydrin, etylene.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Navajo 10275U/4 Concentrate Based In LDPE DescriptionPOLYBATCH® 10275U/4 is a navajo color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabili.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Diamond Polymers NPP 60-3301 Clear Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | |
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 28930 Coax & Telecom Flexible PVC Non-lead stabilized 105C FT-4 riser jacket compound. UV resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Saint-Gobain Meldin® 2001 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |