Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Ovation Polymers Uttap SF 600 Polyethersulfone Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R352AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 901-48/1-F-ISM Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Fiberfil® FV-30 Nylon 6, 30% Glass Reinforced, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina 801-08/98-C-IS Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 828-08/497-Y-RT Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 828-48/27-Y-RT Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | |
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Shinil Chemical SHINCON PPS-CF, Comp. "Y"-1 LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Teknor Apex APEX® RM 8216 Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | DIN 53 479 |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
Specific Gravity | 1.37 - 1.41 g/cc | 1.37 - 1.41 g/cc | ASTM D-792 |
Axiall 9115A Wire & Cable Flexible PVC Low cost tray cable jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.37 - 1.41 g/cc | 1.37 - 1.41 g/cc | ASTM D-792 |
Axiall 19910 Wire & Cable Flexible PVC THHN-THWN, best suited for larger sizes (16 AWG and larger).Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.37 - 1.41 g/cc | 1.37 - 1.41 g/cc | ASTM D-792 |
Axiall 2258 Wire & Cable Flexible PVC TW insulation suitable for 105°C AWM applications. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® GFN 6633 Glass Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |