Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 50/CF/20 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
LG Chemical LUMID HI2202B(W) PA66+GF20%, High Impact Feature: Injection Molding, PA66+GF20%, High ImpactApplication: Automotive (Covers)CAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | |
Momentive Performance Materials TSE322B Heat-Curing Silicone Adhesive, Black RTV6424, RTV6445, and TSE322 silicone adhesives are one-component heat curable silicone adhesive sealants which will bond to many substrates without a primer and which will creep rapidly at elevated.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1/CF/30 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
Techmer ES Electrafil® M-2386 NAT Polycarbonate |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | DBPH Cure |
Shin-Etsu Silicones X-65-130U Electrically Conductive Silicone Elastomer ShinEtsu X65130 U is a black semiconductive silicone compound designed to give very low volume resistivity for molding and extruding. Product Features: Good processability.Lower than average volume .. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | |
Shinil Chemical SHINCON PETG Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® LS-1150G PC/ABS, 15% Glass Filled FR 15% GF reinforcement; can be used in mold frames for LCD BLU.Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.28 g/cc @Temperature 25.0 °C |
1.28 g/cc @Temperature 77.0 °F |
|
Dow Corning MOLYKOTE® 1292 LONG LIFE BEARING GREASE For high-temperature use and applications that come in contact with solvents, fuels and water; recommended for rolling element and plain bearings. Light consistency; resists solvents, fuels and moi.. |
|||
Specific Gravity | 1.28 g/cc @Temperature 25.0 °C |
1.28 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® 9220/55 KIT PARTS A&B 55 Durometer, 2-part, 1 to 1 mix, black Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | |
Colorite Polymers 9511 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | Base |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® LX2801 PC (Asia Pacific) |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ISO 1183 |
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber
(discontinued **) The 30% glass fiber reinforced PPE has an improved dimensional stability, a very high stiffness and heat resistance that allows further uses. |