Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.27 g/cc | 1.27 g/cc | 23/23°C; ASTM D792 |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | 23/23°C; ASTM D792 |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | +.02 |
Spartech 2969-92 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Spartech Spectar® Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Eastman Drystar 0603 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Perstorp Compounds Akestra™ 100 Thermoplastic Copolyester Excellent appearance, clarity, hydrolytic stability, heat resistance and high strength. Used for extrusion and injection molded articles, blow molding, films and sheets. It can be used as a polyst.. |
|||
Specific Gravity | 1.27 - 1.31 g/cc | 1.27 - 1.31 g/cc | ASTM D-792 |
Axiall 8843 Moldings & Extrusions Flexible PVC General purpose, non-lead stabilized extrusion compound. Well suited for 80°C rated automotive tubing.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |