Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.25 g/cc | 1.25 g/cc | |
Radici Heraflex® E 7722 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. High Modulus, Nominal Shore D/15s 69. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
PTS PPE-LXS 314-20 PPE-HIPS, 20% Glass Filled Typical Applications: Water industrial partsInformation provided by PTS LLC. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Specific Gravity | 1.25 - 1.35 g/cc @Thickness 1.57 mm |
1.25 - 1.35 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | |
Lucite International Elvacite ® 2051 Acrylic Resin Elvacite® 2051 is a high molecular weight methyl methacrylate polymer. It is used in many coatings applications providing maximum abrasion resistance, block resistance, and slip. It is non-reacti.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D297, 15 |
Seals Eastern 5401 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Techmer ES Electrafil® NY-3/EC BK PA6 |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 2555-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Samyang Trirex® 3025G10 Polycarbonate, 10% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SFW 5000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Uses: Footwear; General Purpose Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Colorite Polymers CS1524SP Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Colorite Polymers 7772 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | |
Colorite Polymers 8512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 47551 Flexible PVC Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Colorite Polymers 5543 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang. |