Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Nylene® 204 (HS) , Fast Cycle Nylon 6 Description: Nylene® 204 (HS) is a fast cycle, medium viscosity, nucleated nylon 6. 204 is UL approved and automotive approved. Information provided by Custom Resins.ALM, Nylene Canada, and Custom .. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | foam molded; ASTM D792 |
SABIC Innovative Plastics Lexan® FL903 PC Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
PolyOne Edgetek® XT X XT 1001 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
PolyOne Edgetek® NL-08GF-02CF/000 Nylon 6/12, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D1505 |
Honeywell Aegis™ HCA155QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500... |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D1505 |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizedTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D 792 |
MRC Polymers NAXALOYâ„¢ 770-BK272 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
SPS Guang Zhou POLOYâ„¢ 2001(+) PC/ABS Characteristic: Good mechanical properties and good machining propertiesApplications: Electron equipment shell, automobile assorted partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | 23°C; ASTM D792 |
Teknor Apex Flexalloy® 9900-60 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2790 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Teknor Apex Synres® SR 1209A Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ISO 1183 |
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6 Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
Zeon Chemicals Sivic® Z530 Polyblend Nitrile Elastomer Sivic Z530 is a fully fluxed polyblend of 33% ACN NBR/PVC (50/50). It is produced via a mechanical technology, which provides a lump-free homogenous polymer.Improved fuel, ozone, and fire resistance.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
A. Schulman POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE DescriptionPOLYBLAK® Black 4669 is a premium conductive carbon black concentrate containing 35% carbon black based in LLDPE. This carbon black masterbatch is designed to provide smooth extruded su.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
Zylog Hipolyene® 6131 XF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | 15/15°C |
ChevronTexaco Texcool® EXL 300 In service Texcool EXL products provide:A 32,000 hour/8 years of service life with no inhibitor additions neededNo regular inhibitor testing requiredExcellent heat transfer and corrosion protection .. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
E-Polymers TEKAMID® JN2 PPE+PA66 Un-reinforced Chemical resistance PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Specific Gravity | 1.13 g/cc | 1.13 g/cc | @ 25°C |
ACC EP MAP-8.5 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-8.5 contains 8.5% NCO. .. |