Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.091 g/cc | 1.091 g/cc | |
Dow VORANOL™ CP 1421 Polyol VORANOL™ CP 1421 polyol is a polyether polyol especially designed for the production of soft and hypersoft flexible slabstock foams. It is also used at low level (0.5 to around 5 php) as cell open.. |