Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized Acrylonitrile Butadiene Styrene, 5% Glass Reinforced, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | |
Resinlab® CYNERGY CA6605 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Specific Gravity | 1.08 g/cc @Temperature 23.0 °C |
1.08 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | |
Momentive Performance Materials Siloprenâ„¢ Electro 242-15 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | |
Momentive Performance Materials TSE 221-3U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | |
Shin-Etsu Silicones LIMSâ„¢ KE2004-5A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Lubrizol Estane® R180A Thermoplastic Polyurethane Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Ensinger TECANYL™ MT Autoclavable Polymer TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Ensinger TECANYL™ MT XRO Autoclavable Polymer TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | 23°C; ASTM D792 |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | 23°C; ASTM D792 |
Asahi Kasei Xyron® 340Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | 23°C; ASTM D792 |
Asahi Kasei Xyron® 500V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ISO 1183 |
Azoty Tarnow™ Tarnamid® T-27 MCS HI Polyamide 6 - Impact Modified Very high impact resistance, cold impact grade (to -40°C). Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has t.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ISO 1183 |
Ascend Performance Materials Vydyne® 41 Nylon 66, Conditioned Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM 792 |
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase |
|||
Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
E-Polymers SEPAZ® N3040HR Nanoclay 3% Dimensional stability, Super Toughness Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |