Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
PolyOne Maxxam™ PPH-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Polymax® Maxelast® P2845 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Polymax® Maxelast® P2865 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ISO 1183 |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Radici Radilon® A USZ200 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Momentive Performance Materials RTV6703 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® BM-0320 J ABS, Unreinforced Heat resistantInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® SD-0150AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Supreme Petrochem SP6432 9690 Medium Impact Polystyrene Characteristics High flow Good toughness Available in various colors Processing Injection moldingApplications Air conditioner and cooler grills Refrigerator parts Washing machine components Mate.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Chase Plastics CP Pryme® A100 ABS Molding Resin Information provided by Chase Plastics. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 1.04 g/cc @Temperature 25.0 °C |
1.04 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® SL 10 RELEASE MODIFIER Olefin-free; low viscosityInformation provided by Dow Corning |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
ELASTO UK Dryflex® 402901S SBS Based Material, 90A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® 8038N Thermoplastic Elastomer Elastocon® 8038N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8038N is FDA compliant and well suited.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Diamond Polymers ABS 9500B Description: Blow Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Asahi Kasei Thermylene® P6-20FG-1740 20% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Americas Styrenics EC6600 High Impact Polystyrene Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy.. |
|||
Specific Gravity | 1.04 - 1.07 g/cc | 1.04 - 1.07 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 2009 GK (B) BLK Polypropylene, 20% Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® EG-0763 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Supreme Petrochem SP201 4551 Light Stabilized Polystyrene Characteristics Excellent light stability to fluorescent & incandescent light sources Very high clarity and heat resistance Excellent strength & stiffness Processing Injection molding Extrusion A.. |
|||
Specific Gravity | 1.04 g/cc @Temperature 25.0 °C |
1.04 g/cc @Temperature 77.0 °F |
|
Dow Corning 29 Additive Enhances flow, leveling and gloss; also imparts mar resistance and anti-blocking.Information provided by Dow Corning |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ISO 2782 |
AlphaGary Evoprene™ GC 5658 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |