Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.018 - 1.038 g/cc | 1.018 - 1.038 g/cc | ASTM D1298 |
Reltek BONDiT™ C-52 Bonding Agent, Adhesive and Primer Key PropertiesAdhesion promoter and primer for molding thermoplastics, such as polyethyleneApplicationsPrimer and adhesion promoter on various substrates for polyolefin, fluoropolymers (other than P.. |
|||
Specific Gravity | 1.018 - 1.038 g/cc | 1.018 - 1.038 g/cc | ASTM D1298 |
Reltek BONDiT™ C-6 Bonding Agent, Adhesive and Primer Key PropertiesAdhesion promoter and primer for molding polyurethane and rubberApplicationsHigh functionality produces good bond strength in bonding difficult-to-bond substrates, such as polyethylene.. |
|||
Specific Gravity | 1.018 - 1.038 g/cc | 1.018 - 1.038 g/cc | ASTM D1298 |
Reltek SEALiT™ A-46 Clear Coat & Sealant Key Properties: Optical clear coat for metals, glass and ceramic.Sealant for ceramic, electronic components (e.g. flex-PCB’s exposed to moisture).Architectural coating.Applications: Handles continu.. |
|||
Specific Gravity | 1.018 - 1.038 g/cc | 1.018 - 1.038 g/cc | ASTM D1298 |
Reltek BONDiT™ A-3 Bonding Agent, Primer and Adhesive Key Properties: Adhesion promoter and primer for coatings, sealants and adhesives on metals, glass and ceramic.Exceptional moisture and high pH resistance.Outstanding harsh environment protection an.. |
|||
Specific Gravity | 1.018 - 1.038 g/cc | 1.018 - 1.038 g/cc | ASTM D1298 |
Reltek BONDiT™ A-43 Bonding Agent, Primer and Adhesive Key Properties: Adhesion promoter for most thermoplastics, thermoset materials, elastomers, polyurethanes.Can be used on metals, glass and ceramicApplications: High functionality produces good bond .. |
|||
Specific Gravity | 1.018 g/cc | 1.018 g/cc | |
Esstech X-844-7469 2-Methoxyethoxyethyl Methacrylate, C9H16O4 MOEOEMA is a methacrylate with a variety of applications including: coatings, pressure sensitive adhesives and cosmetics. Listed on the Toxic Substance Control Act List. CAS # 45103-58-0.Informati.. |
|||
Specific Gravity | 1.018 g/cc | 1.018 g/cc | |
Dow SPECFLEX™ NC 638 Polyol SPECFLEX™ NC 632 polyol is a specialty capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082-00-2 0.. |
|||
Specific Gravity | 1.018 g/cc | 1.018 g/cc | |
Dow VORANOL™ 4701 Polyether Polyol VORANOL™ 4701 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.Informa.. |