Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.017 g/cc | 1.017 g/cc | |
Northstar Polymers BNA-005 Polyester Curing Agent Information provided by Northstar Polymers. |
|||
Specific Gravity | 1.017 g/cc | 1.017 g/cc | |
Struktol V-PEAS LA LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING STRUKTOL® V-PEAS LA is a very effective lubricant with externally lubricating properties which has no negative impact on clarity in extrusion, calendering, or injection molding. STRUKTOL® V-PE.. |
|||
Specific Gravity | 1.017 g/cc | 1.017 g/cc | |
Struktol V-PEAS Processing Additive Polymeric complex ester of saturated fatty acids.Typical Applications: STRUKTOL® V-PEAS is a very compatible complex ester lubricant. It has noted performance in clear–calendared sheet. It a.. |
|||
Specific Gravity | 1.017 g/cc | 1.017 g/cc | |
Dow VORANOL™ 4815 Polyether Polyol VORANOL™ 4815 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.Informa.. |