Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.975 g/cc | 0.975 g/cc | ASTM 792 |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning Q7-2243 LVA Simethicone USP Dow Corning® Q7-2243 LVA, Simethicone USP is a specially formulated low volatile silicone antifoam for use in various medical and pharmaceutical applications. Especially advantageous in the manufac.. |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7137 HIGH SPEED CROSSLINKER Syl-Off® 7137 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issueInformation provided by.. |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7138 HIGH SPEED CROSSLINKER Syl-Off® 7138 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue, and Syl-Off® 7678 Cr.. |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® PMCP7137 High Speed Crosslinker Syl-Off® 7137 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue.Information provided b.. |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® PMCP7138 High Speed Crosslinker Syl-Off® 7137 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue, and Syl-Off® 7678 Cr.. |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPOHX-4010 Polymer 4000CS Is chemically equivalent to DOW CORNING® 3-0213 POLYMER, 4000CS. Polydimethylsiloxane polymer with terminated, curable silanol functionality, viscosity = 4,000 cp.Information provided by Dow Cornin.. |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 10,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 10,000CS. 100% active, 10,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 12,500CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 12,500CS. 100% active, 12,500 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 5,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 5,000CS. 100% active, high viscosity, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning 3-3602 Polymer 80,000 CS Polydimethylsiloxane polymer with terminated, curable silanol functionality, viscosity= 80,000 cp.Information provided by Dow Corning |
|||
Specific Gravity | 0.975 g/cc @Temperature 25.0 °C |
0.975 g/cc @Temperature 77.0 °F |
|
Dow Corning 54 Additive Provides mar resistance, slip, leveling and gloss. Also aids in pigment dispersion.Information provided by Dow Corning |