Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.942 - 0.945 g/cc | 0.942 - 0.945 g/cc | ASTM D1505 |
LG Chemical SEETEC PH150 HDPE Blown Film Grade Features: Characteristics : Excellent weather resistance & Environmental stress cracking resistanceAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 20.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM 792 |
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM 792 |
Multibase Multi-Flex® D 5308 X Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM 792 |
Multibase Multi-Flex® G 7430 TPE Styrene Ethylene Butylene Styrene Block Copolymer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM 792 |
Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-88-N882-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ISO 1183 |
Total MDPE HR 515 Medium Density Polyethylene, Blown Film MDPE HR 515 is a medium density polyethylene produced with hexene as a co-monomer. It shows a broad molecular weight distribution ensuring outstanding processability.MDPE HR 515 is especially dedic.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Specific Gravity | 0.942 g/cc | 0.942 g/cc | ASTM D792 |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |