Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® C4730 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® C4740 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® C4750 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® C4760 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® P1960T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® P1985NT TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® P1985T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® P3965H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® D6965H TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Polymax® Maxelast® P1957TA TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | 20/20°C |
LyondellBasell DPNB Dipropylene glycol normal butyl ether Information provided by Lyondell. |
|||
Specific Gravity | 0.912 - 0.916 g/cc | 0.912 - 0.916 g/cc | ASTM D1505 |
LG Chemical SEETEC ST508 Linear Low Density Polyethylene, Cast Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM 792 |
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM 792 |
Multibase Multi-Flex® A 7202 MR TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM 792 |
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1249D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.912 g/cc | 0.912 g/cc | ASTM D792 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.912 g/cc @Temperature 25.0 °C |
0.912 g/cc @Temperature 77.0 °F |
|
Dow Corning 203 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |