Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products P251-01 Polypropylene Copolymer, Black Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | |
Mapal Plastics Maplon Type D Polypropylene Sheet Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
LTL Color Compounds ColorRxâ„¢ PP1-2005ARX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All in.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ISO 2781 |
Kraton® G1701 E (SEP) Linear Diblock Copolymer Description: Kraton G1701 E is a clear linear diblock copolymer based on styrene and ethylene/propylene, S-E/P, with bound styrene of 35% mass. It is supplied from Europe in the product form identif.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D4025 |
Kraton® G1726 M (SEBS) Linear Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Lucent Polymers PPC-210 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 55-9000 TPE Product Description: StarGrip GP 55-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2264B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1097F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P701J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | |
Teknor Apex Tekbond® TB 1158A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green P30336 Concentrate Based In Homopolymer PP DescriptionPOLYBATCH® P30336 is a green color concentrate based in Homopolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P30244/4 is typically .. |
|||
Specific Gravity | 0.910 - 0.920 g/cc | 0.910 - 0.920 g/cc | |
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed Product Description: Epolene C-26 is a maleic anhydride grafted polyethylene coupling agent for polyethylene (PE) composites. The polar functionality and molecular weight are optimized to provide ba.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-11P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Information provided by Westlake Chemical |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green P30336 Concentrate Based In Homopolymer PP DescriptionPOLYBATCH® P30336 is a green color concentrate based in Homopolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P30244/4 is typically .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Cheng Yu Plastic PP225 Flame Retardant Polypropylene, Medium Impact |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 15°C; ASTM D1298 |
ExxonMobil Gargoyle Arctic 300 Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity a.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D4025 |
Kraton® G1726 M (SEBS) Linear Triblock Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1875HF Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
PolyOne Synprene® RT-3605 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingInformation provided by PolyOne.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | <= 0.910 g/cc | <= 0.910 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |