Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.9035 g/cc | 0.9035 g/cc | |
ChevronTexaco ParaMountâ„¢ ELV Paraffinic Process Oil FeaturesChevron ParaMount ELV Paraffinic Process Oil offers all the advantages of a bright stock including low weight loss and excellent solubility.ELV is exceptional because of its very light color.. |