Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.903 g/cc | 0.903 g/cc | 23/23°C; ASTM D792 |
M. Holland Company CP503 Polypropylene Impact Copolymer Impact copolymerGood impact resistanceLow temperature impact resistanceApplications: Compounding |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D1505 |
LG Chemical LC100 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.903 g/cc @Temperature 25.0 °C |
0.903 g/cc @Temperature 77.0 °F |
|
Dow Corning Z-6518 SILANE Dow Corning® Z-6518 Silane is an organofunctional reactive silane. The product have a vinyl reactive organic group and a trimethoxysilyl or triethoxysilyl reactive inorganic group. Dow Corning® Z-.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | 15°C |
ExxonMobil 512 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Specific Gravity | 0.903 g/cc | 0.903 g/cc | 15°C |
ExxonMobil 512 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |