Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE) Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE) Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
Network Polymers Softflex® 5500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good .. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Elastamax™ XL 0135-33 Styrene Butadiene Block Copolymer (SBC) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2701C Thermoplastic Elastomer (TPE) Dynaflex™ G2701C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Rubbery Feel.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Dynalloy™ OBC8200-BT50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8200-BT50 is a translucent grade to be used in blow molding applications. New Product. Commercial specifications have not been established. - Excellent Colorability - Rubbery FeelPurge.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Synprene® RT-3850MS Styrene Butadiene Block Copolymer (SBC)
(discontinued **) |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Synprene® RT-3870M Styrene Butadiene Block Copolymer (SBC)
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
PolyOne Synprene® RT-3880M Styrene Butadiene Block Copolymer (SBC)
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Specific Gravity | 0.898 g/cc | 0.898 g/cc | 20/20°C |
LyondellBasell PE Propylene glycol ethyl ether Information provided by Lyondell. |