Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D1505 |
LG Chemical LC170 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D1505 |
LG Chemical LC370 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Specific Gravity | 0.870 - 0.910 g/cc | 0.870 - 0.910 g/cc | BAM 1014 |
Kraton® G2806 GO-N (SEBS) Compound Description: Kraton G2806 GO-N is a compound designed for film applications in the Personal Care market: Kraton G2806 GO-N - supplied as an organic dusted dense pelletRegion: Asia Pacific, Europe, J.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 2313 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1672A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1880 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1900-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2137 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 630 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 632 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 634 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D1298 |
ExxonMobil 763 Mobilmet 760 Series Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15.6°C; ASTM D4052 |
ExxonMobil 846 Mobil DTE 800 Series Mobil DTE 832 and 846 are superior performance turbine oils designed for use in steam turbines, gas turbines and combined cycle gas turbine (CCGT) applications under the most severe operating condit.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 32 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Specific Gravity | 0.870 g/cc @Temperature 25.0 °C |
0.870 g/cc @Temperature 77.0 °F |
|
Dow Corning MOLYKOTE® G-4700 EXTREME PRESSURE SYNTHETIC GREASE Synthetic (PAO) extreme pressure greaseFeatures: Long-term lubrication for moderate loads at higher speeds, especially for food-contact applications for where a white grease Is preferred. Formulate.. |
|||
Specific Gravity | 0.870 g/cc @Temperature 25.0 °C |
0.870 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 2CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 2CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications. INCI Name: DimethiconeInf.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D1505 |
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | |
ChevronTexaco Superla® 50 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | Part B |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | Part B |
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 634 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 639 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D1298 |
ExxonMobil 762 Mobilmet 760 Series Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro.. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 630 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 632 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | 15°C; ASTM D4052 |
ExxonMobil 636 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | |
Abatron Abosolv™ General Purpose Thinner and Solvent Abosolv™ is a solvent for LiquidWood®: for thinning the product and cleaning up. Abosolv™ can be added to LiquidWood® up to 1 part Abosolv™ to 1 part LiquidWood® by volume. |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D792 |
Teknor Apex MONPRENE® MP 2137 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.870 g/cc | 0.870 g/cc | ASTM D1505 |
LG Chemical LC175 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |