Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.869 - 0.873 g/cc | 0.869 - 0.873 g/cc | ASTM D3505 |
LG Chemical Toluene Colorless liquid with benzene odor, Heavier than air and highly inflammable, and Not soluble to water, Readily soluble in alcohol and etherStructure & Characteristics: C6H5CH3. Synthesized by extrac.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 15°C; ASTM D1298 |
ExxonMobil 424 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 15.6°C; ASTM D4.52 |
ExxonMobil 150 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 15.6°C; ASTM D4.52 |
ExxonMobil 150 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 15°C; ASTM D1298 |
ExxonMobil 424 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil Vactra 1 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 60°F |
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar GEO Oil is a high-quality, non-detergent, ashless gas engine oil designed primarily for use in Ajax 2-stroke cycle natural gas engines. The SAE 15W-40 viscosity grade meets the low-t.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 60°F |
ConocoPhillips El Mar® 2000 Oil SAE Grade 15W-40 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Specific Gravity | 0.869 g/cc | 0.869 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil Vactra 1 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |