Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.700 g/cc | 0.700 g/cc | Uncured |
Permabond CSA Cyanoacrylate Surface Activator Permabond C Surface Activator (CSA) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It also enables fillets of cu.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | |
Technetics Group PLASTOLON™ Low Density PTFE Tape
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | |
Shin-Etsu Silicones X-33-156-5 Silicone Primer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.004" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.005" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.006" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.008" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.010" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Specific Gravity | 0.700 g/cc @Temperature 25.0 °C |
0.700 g/cc @Temperature 77.0 °F |
|
Dow Corning HV 10 PRIMER Adhesion to aluminium, stainless steel, galvanised steel, epoxy-glass fibre, PFA, good with addition cured silicone rubbers.Information provided by Dow Corning |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | |
Chesterton 276 Electronic Component Cleaner Description: Chesterton® 276 Electronic Component Cleaner is a fast acting, industrial strength cleaner containing zero ozone depleting potential. It is a high performance, non-chlorinated product .. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | |
Chesterton 277 Metal Surface Degreaser Description: Chesterton® 277 Metal Surface Degreaser is a fast acting, industrial strength cleaner containing zero ozone depleting potential. It is a high performance, non-chlorinated product desig.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | |
Chesterton 660 Silicone Lubricant Description: Chesterton® 660 Silicone Lubricant is a clean, clear, silicone fluid which will provide continuous film lubrication for mechanical parts and sliding surfaces constructed of plastic, ru.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | ASTM D3574 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Specific Gravity | 0.700 - 0.800 g/cc | 0.700 - 0.800 g/cc | |
BCC Products BC 37 Ceramic Microspheres BC 37 are hollow microspheres, which are ceramic in nature. They are an efficient lightweight filler material to be used in applications with most resins.Information provided by BCC Products, Inc. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | Uncured |
Permabond A905 Anaerobic Surface Activator Permabond A Surface Activator (A905) is used in conjunction with Permabond A (anaerobic) adhesives and sealants. A905 is designed to allow non-metallic surfaces to be bonded/sealed. It also accelera.. |
|||
Specific Gravity | 0.700 g/cc | 0.700 g/cc | |
Chesterton 677 Dry Lubricant Description: When lubricated areas must be free of oil and oily stains, Chesterton® 677 Dry Lubricant is the product of choice. It is a clean, dry, multi-purpose, high-quality, PTFE-based powder lu.. |