Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.240 g/cc | 0.240 g/cc | ASTM D3574 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Specific Gravity | 0.240 g/cc | 0.240 g/cc | ASTM D3574 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Specific Gravity | 0.240 g/cc | 0.240 g/cc | |
BCC Products MB 1150 Polyurethane Foam Modeling Board MB 1150 is an Avocado colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1150 is low density foam of approximately 15lbs/ft3 board. Easily cut using CNC machining equipment o.. |