Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3550 cP @Temperature 190 °C |
3550 cP @Temperature 374 °F |
ASTM D3226 |
Westlake Epolene® C-10 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-10 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc.. |