Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 48.0 - 610 cm | 18.9 - 240 in | Average value: 163 cm Grade Count:10 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |