Polymer Property : Spiral Flow = 6.10 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 15.5 cm
6.10 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
LyondellBasell Alathon® M6028 High Density Polyethylene
ApplicationsM 6028 is a homopolymer that is warp resistant, exhibits excellent toughness, stiffness and color as well as low odor and good processing stability. Typical applications include safety ..
Spiral Flow 15.5 - 55.8 cm
6.10 - 22.0 in
Average value: 33.6 cm Grade Count:39
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..