Polymer Property : Spiral Flow = 55.1 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 140 cm
55.1 in
175°C/1000 psi
Cookson Group Plaskon® SMT-B-1 LAS (146.408) Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA) requiring low alpha particle count. It is formulated ..