Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 95.0 cm | 37.4 in | |
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Spiral Flow | 95.0 - 117 cm | 37.4 - 46.1 in | Average value: 99.2 cm Grade Count:9 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Spiral Flow | 95.0 cm @Thickness 2.00 mm, Temperature 250 °C |
37.4 in @Thickness 0.0787 in, Temperature 482 °F |
Borealis Method |
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st.. |
|||
Spiral Flow | 95.0 cm | 37.4 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Spiral Flow | 95.0 cm | 37.4 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |