Physical Properties Metric English Comments
Spiral Flow 87.0 cm
34.3 in
Cross Section: 7[mm]x3.5[mm]; AKRO
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..