Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 83.0 cm | 32.7 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |