Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 73.66 cm @Temperature 260 °C |
29.00 in @Temperature 500 °F |
10 ips,3.175 X 1524 mm |
SABIC Innovative Plastics Cycolac® BDT5510 ABS Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only. |