Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 44.0 - 45.0 cm @Temperature 220 - 220 °C |
17.3 - 17.7 in @Temperature 428 - 428 °F |
Average value: 44.5 cm Grade Count:2 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Spiral Flow | 44.0 cm @Temperature 220 °C |
17.3 in @Temperature 428 °F |
ASTM D3123 |
Total PSI 3341 High Impact Polystyrene Total Petrochemicals Polystyrene 3341 is a high impact polystyrene for the extrusion industry. Its good mechanical and thermal properties leads to the production of thermoformed articles of good ri.. |