Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 36.0 cm | 14.2 in | NOVA Snake Flow Test |
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer. |
|||
Spiral Flow | 36.0 cm | 14.2 in | NOVA Snake Flow Test |
NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties.Applications: Food containers and lids, frozen food containers.Dat.. |
|||
Spiral Flow | 36.0 - 45.0 cm | 14.2 - 17.7 in | Average value: 41.0 cm Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Spiral Flow | 36.0 cm | 14.2 in | Exxon Method |
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Impact, Good Stiffness, Excellent ESCRUses: Pails, Industrial containers, Structural foams |
|||
Spiral Flow | 36.1 cm | 14.2 in | Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar |
LyondellBasell Alathon® H5520 High Density Polyethylene ApplicationsALATHON H 5520 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include house.. |
|||
Spiral Flow | 36.0 cm | 14.2 in | NOVA Snake Flow Test |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |