Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 34.0 - 50.0 cm | 13.4 - 19.7 in | Average value: 43.8 cm Grade Count:12 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Spiral Flow | 34.0 - 56.0 cm @Temperature 220 - 260 °C |
13.4 - 22.0 in @Temperature 428 - 500 °F |
Average value: 45.8 cm Grade Count:5 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |