Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 3.60 cm | 1.42 in | |
Tipco Tipcolite® TCF 1132 - CNSL+Mineral Modified Phenolic Resin having 36mm Norton Flow with 7% Hexamine CNSL/Mineral Modified Phenolic Resin having 36mm Norton Flow, in Powder FormApplications: Nitrile RubberProcessing: CompoundingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |