Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 35.0 - 700 cm | 13.8 - 276 in | Average value: 110 cm Grade Count:10 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |