Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 36.0 - 45.0 cm | 14.2 - 17.7 in | Average value: 41.0 cm Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Spiral Flow | 44.0 - 45.0 cm @Temperature 220 - 220 °C |
17.3 - 17.7 in @Temperature 428 - 428 °F |
Average value: 44.5 cm Grade Count:2 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Spiral Flow | 35.0 - 45.0 cm | 13.8 - 17.7 in | Average value: 41.3 cm Grade Count:8 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |