Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 92.0 - 105 cm | 36.2 - 41.3 in | 177°C/1000 psi |
Cookson Group Plaskon® SMT-B-1FX (146.801) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It is a reduced catalyst version of SMT-B-1F and provide.. |
|||
Spiral Flow | 104 - 105 cm | 40.9 - 41.3 in | Average value: 104 cm Grade Count:4 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |