Spiral Flow 53.8 cm
21.2 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
LyondellBasell Alathon® ETP H5057 High Density Polyethylene
ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavit..