Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 43.0 - 62.0 cm @Temperature 220 - 220 °C |
16.9 - 24.4 in @Temperature 428 - 428 °F |
Average value: 51.9 cm Grade Count:7 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Spiral Flow | 43.0 cm @Temperature 220 °C |
16.9 in @Temperature 428 °F |
ASTM D3123 |
Total PSI 2451 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 2451 is a high heat resistance, impact polystyrene for injection blow molding, thermoforming. It is recommended for the manufacturing of articles which require good.. |
|||
Spiral Flow | 43.0 cm | 16.9 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |