Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 4.20 cm | 1.65 in | |
Tipco Tipcolite® TPF 1317 - Unreinforced Phenolic Resin with Minerals having 42 mm Norton Flow with 9% Hexamine Phenolic Resin with Minerals having 42mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd.,