Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Spiral Flow = 34.0 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 34.0 - 50.0 cm
13.4 - 19.7 in
Average value: 43.8 cm Grade Count:12
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Spiral Flow 34.0 - 56.0 cm

@Temperature 220 - 260 °C
13.4 - 22.0 in

@Temperature 428 - 500 °F
Average value: 45.8 cm Grade Count:5
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..