Polymer Property : Linear Mold Shrinkage, Flow = 0.0073 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0065 - 0.0073 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0073 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Linear Mold Shrinkage, Flow 0.0065 - 0.0073 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0073 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0065 - 0.0073 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0073 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Linear Mold Shrinkage, Flow 0.0065 - 0.0073 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0073 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0065 - 0.0073 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0073 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.